    FAQ > There's no such thing as a dumb Question! > Is there ASTM Standrds for Electropolishing and Passivating?

    Search the FAQ for entries containing:

    Yes! for Electropolishing it is ASTM-B912

     For passivating it is ASTM-A967

     For Cleaning, Descaling, Pickling it is ASTM-A380